03-24-2020, 01:59 AM
my steps, i would do in this situation:
- cleaning the build plate and the fep (inner and outer) with IPA
- sticking capton tape around the lcd and clean the lcd (dry towel)
- leveling with a stack of two pieces of paper (witout the vat)
- rotate one of the parts to get a bigger surface on build plate
- increase the exposure time (a little) up to 80sec base and 10 sec layers
but this is only my way to check ;-)
- cleaning the build plate and the fep (inner and outer) with IPA
- sticking capton tape around the lcd and clean the lcd (dry towel)
- leveling with a stack of two pieces of paper (witout the vat)
- rotate one of the parts to get a bigger surface on build plate
- increase the exposure time (a little) up to 80sec base and 10 sec layers