Hi everyone,

For the 15 days since I bought it it has always printed beautifully with the test resin.

Mars 4 ultra 9k model
8k rapid white smoke resin

I printed from the beginning with the basic parameters

I upload the files to chitubox and put the supports
slice and load wi fi directly on the printer

Since yesterday it has printed the base for me and then nothing more.

The base remains glued to the resin plate while there is nothing on the platform.

I don't know how to explain it because I haven't changed anything.

The only thing is the outside temperature which was cold for a few days but today for example it is again at 18-20 degrees outside
Double supports as in the image.

I attach images of the print setting and supports
I wouldn't know what to change honestly.