01-28-2021, 06:58 PM
tHE onlt "too much" platen adhesion prolem I have expedrienced was with that damned useless 'water washable' resin. I wrote a nasty reveiw on Amazon and Elegoo contacted me offedring a 1 liter bottle of any resin I wanted--i.e. they know it's garbage--read more about my experiences with it here.
80 grit is pretty harsh--I had purchased a "Pro" platen to experiment with and roughed it up "just a bit" with 180 grit using a random orbit sander. I had to use an 8" coarse wire wheel in a 3600 rpm bench grinder to get that damned water washable crap off the plate...
80 grit is pretty harsh--I had purchased a "Pro" platen to experiment with and roughed it up "just a bit" with 180 grit using a random orbit sander. I had to use an 8" coarse wire wheel in a 3600 rpm bench grinder to get that damned water washable crap off the plate...